873 writing effect suede feeling yangbuck resin
1.Application:PU yangbuck resin
2.Product data
Appearance:milky white liquid
Solvent: MEK/TOL
Viscosity(mPa·s/25℃):2000-5000
Solid content(%): 20±2
3.Property
good writing effect suede feeling effect after tumbling
4.Operation
①directly add color powder into yangbuck resin and stir
② PU base direct coating →PU yangbuck resin(coating with the clearance of 0.18-0.2mm )yangbuck foaming drying 2-3 mins, foaming temperature 170~175℃→ tumbling and other treatments (the more coating of the more rough surface after drying,on the contrary smaller foam,please testing by yourself.)
③foaming 2-3 mins under 170~175℃, after dying it can bee printing pattern or hand feeling treating.
5. Caution notes
①please test the dissolvent between 873 and pigment if need the color changing work.
②please stir it before using
③Store it in dark place sealed
④It can be stored for 3 months without change in quality
6.Package:180kg/drum